| Mn | Manganese foil measured at NSLS X23A2 February 29 2008 by BR |
| Fe | Iron foil measured at NSLS X11A 10/4/2002 by BR |
| Goethite | Goethite (Fe3+) powder on kapton tape, measured by Shelly Kelly, BR, Max Boyanov, Ken Kemner, APS 10ID March 2005 |
| Hematite | Hematite (Fe3+) powder on kapton tape, measured by Shelly Kelly, BR, Max Boyanov, Ken Kemner, APS 10ID March 2005 |
| Lepidocrocite | Lepidocrocite (Fe3+) powder on kapton tape, measured by Shelly Kelly, BR, Max Boyanov, Ken Kemner, APS 10ID March 2005 |
| Co | Cobalt foil measured at NSLS X11B November 2003 by BR |
| Ni | Nickel foil, focused, detuned 50%, measured at APS 13ID June 2001 |
| Cu | copper foil 150K measured at NSLS X11A, Sep. 1992, Matt Newville, Yanjun Zhang, BR |
| Zn | Zinc foil measured at NSLS X11B November 2003 by BR |
| Realgar | AsS powder on tape, unfocused, detuned 75%, clockwise at E=12000eV, SSRL 2-3, 10K, April 1997 |
| Zr | Zirconium foil measured at NSLS X11B November 2003 by BR |
| Nb | Niobium foil measured at NSLS X11B July 2004 by BR |
| Mo | Molybdinum foil measured at NSLS X11B November 2003 by BR |
| Rh | Rhodium foil measured at NSLS X11B July 2004 by BR |
| Ag | Gold foil measured at APS 20BM 7/1/2006 by BR |
| Cd | Cadmium foil measured at APS 10ID 18 Nov 2006 by BR |
| Pt | Platinum foil measured at NSLS X11B July 2004 by BR |
| Au | Gold foil measured at APS 20BM 10/29/2005 by BR |
| U4 | UO2 nanoparticles, reduced from U6 by green rust in a wet paste, sample made by Ed OLoughlin, measured by Shelly Kelly, Max Boyanov, Ken Kemner at APS 10ID, 3/14/2006 |
| U6 | Hydrated uranyl phosphate diluted in boron nitride, prepared by Shelly Kelly, measured by Shelly Kelly, BR, Max Boyanov, Ken Kemner, APS 10ID March 2006 |